Hey guys, here is an update on my HHO gen.
Here is three of the seven cells
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30402.jpg)
The plates are 304 stainless 4" x 9" 18g
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30403.jpg)
I sanded the plates horizontal then vertical
I also threw together a test cell for fun.
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30401.jpg)
How come when i turn it on the negative gets very hot and starts to melt?
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30400.jpg)
I haven't found any thing to build the container out of yet, any suggestions?
Does everything look ok thus far?
Thanks,
Alex
Here is three of the seven cells
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30402.jpg)
The plates are 304 stainless 4" x 9" 18g
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30403.jpg)
I sanded the plates horizontal then vertical
I also threw together a test cell for fun.
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30401.jpg)
How come when i turn it on the negative gets very hot and starts to melt?
![](http://i297.photobucket.com/albums/mm220/09aslattery/SNV30400.jpg)
I haven't found any thing to build the container out of yet, any suggestions?
Does everything look ok thus far?
Thanks,
![Thank You](http://www.energeticforum.com/core/images/smilies/thanks.gif)
Alex
Comment